Quality Diagnostics · D04

Chipping

Chipping
Ceramic injection molding reference component

Symptom: localized material loss at an edge, corner, or detail feature - can occur during demolding, handling, or ball-mill polishing.

StageTraceability Signature
DemoldingChip location near an undercut or ejector point, from insufficient green-body strength
HandlingChip location random - micro-impacts in the green state
Ball-mill polishingChips mostly on thin-wall edges, from polishing-media impact